The other thing you can do is get the manifold extrude honed then take an abrasive roll (about 50 grit) and just lightly rough up the last few inches of the runner after the water injection point. That is where the water wetting would be an issue and this sort of surface roughning is frequently used by professional porters to solve that problem.